So, I'm looking for an inexpensive supply of steel hands to practice heat bluing with.

Looking at esslinger.com, there are lots of "silver" hands available for a reasonable price. E.g.: 114 Piece White Multi-Style Watch Hands, White Dauphine Style Hour and Minute Hands, etc.

There are also, of course, a myriad of cheap silver Chinese hands available on eBay.

Does anyone know what metal inexpensive "silver" hands are typically made out of? I'm very, very new to this, and honestly don't know whether hands are typically steel, anodized aluminum, or whatever ...

Thanks in advance for any tips and advice!

Link to comment
Share on other sites

2 hours ago, dpn said:

So, I'm looking for an inexpensive supply of steel hands to practice heat bluing with.

Looking at esslinger.com, there are lots of "silver" hands available for a reasonable price. E.g.: 114 Piece White Multi-Style Watch Hands, White Dauphine Style Hour and Minute Hands, etc.

There are also, of course, a myriad of cheap silver Chinese hands available on eBay.

Does anyone know what metal inexpensive "silver" hands are typically made out of? I'm very, very new to this, and honestly don't know whether hands are typically steel, anodized aluminum, or whatever ...

Thanks in advance for any tips and advice!

Steel is what you want. Preferably stainless. Get a magnet- good quality 304, 306, 316 stainless alloy will be non magnetic. Try ofrei and kas-ker. otherwise vintage NOS is always good but like we talked about-can get spendy. 

Otherwise some can be cheap tin or aluminium. Even plastic. 

  • Like 1
Link to comment
Share on other sites

Stainless steel won't blue; I don't know of any watch hands being made of it either.

If the supplier doesn't state or know the material check them with a magnet. Hands can be almost any material from gold to plastic but brass and steel are the most common.

  • Like 1
Link to comment
Share on other sites

3 hours ago, nickelsilver said:

Stainless steel won't blue; I don't know of any watch hands being made of it either.

If the supplier doesn't state or know the material check them with a magnet. Hands can be almost any material from gold to plastic but brass and steel are the most common.

Yeah, they're out there. All modern day stuff. Micro brands.   Depending what grade and carbon content they contain  they will turn color tho. Manufcrs. don't list the grades tho lol. Just keep my trusty magnet handy. melted a plastic set once..

Link to comment
Share on other sites

I've got my propane torch, my IR thermometer, my brass scarf, my brass heating box, and my polishing stuff all either here or on the way. 

I honestly didn't think that finding steel hands was going to be the hard part! *grin*

I can practice a lot with screws and old blued hands, but if I want to actually make usable hands I'm going to need to figure out a supplier.

Interestingly, Esslinger has been super quick to reply to my parts inquiries. My inquiry about what makes up their "silver" hands has been met with silence, so I agree they're likely to be some kind of mystery anodized or coated base metal.

This has been, and will continue to be, a fascinating exercise. I'm going to be cross-posting on the NAWCC forums, since there's a lot of good heat-bluing info there. Maybe someone will have a good supplier they'll be willing to share.

Link to comment
Share on other sites

The better the quality of the steel and with practice the better the bluing will be, you should have an even blue colour all the same. I always quenched clock hands and screws in oil, it would give a shine look and not a dull finish.  

Link to comment
Share on other sites

8 hours ago, dpn said:

I've got my propane torch, my IR thermometer, my brass scarf, my brass heating box, and my polishing stuff all either here or on the way. 

I honestly didn't think that finding steel hands was going to be the hard part! *grin*

I can practice a lot with screws and old blued hands, but if I want to actually make usable hands I'm going to need to figure out a supplier.

Interestingly, Esslinger has been super quick to reply to my parts inquiries. My inquiry about what makes up their "silver" hands has been met with silence, so I agree they're likely to be some kind of mystery anodized or coated base metal.

This has been, and will continue to be, a fascinating exercise. I'm going to be cross-posting on the NAWCC forums, since there's a lot of good heat-bluing info there. Maybe someone will have a good supplier they'll be willing to share.

Where did you find the swarf and heat tray?

Link to comment
Share on other sites

7 hours ago, oldhippy said:

same. I always quenched clock hands and screws in oil, it would give a shine look and not a dull finish.  

Do you every get the black tar-like crud on them when you do this? Ever had and luck with just air cool down?

Link to comment
Share on other sites

If its screws after they have be cleaned and polished, I would put them in an old watch cleaning machine to make sure all dirt got completely removed, crud can be caused by bluing something that still has dirt or grease on it. Hands would be washed in soft soap and warm water and dried in a lint free cloth before bluing. 

Link to comment
Share on other sites



  • Recently Browsing

    • No registered users viewing this page.
  • Topics

  • Posts

    • Yes and no. I use Moebius 9501 synthetic grease and it is significantly runnier than the Moebius 9504 synthetic grease (and I assume Molykote DX) that I previously used. I haven't seen 9504 spread and it is in my opinion the best grease money can buy. However, my current method of cleaning doesn't remove it from the parts, so that's why I have decided to use the 9501 instead. I believe I read somewhere that Molykote DX too is difficult to clean off. Thinking about it, I'm pretty sure my 9501 grease which expired in June 2022 is runnier now than it was when it was new, but whether new or old it always needs to be stirred before use. So, that's why I treat the parts of the keyless works, cannon pinion, etc. with epilame. That was very thoughtful of you and something that had completely passed me by. Not sure what the epilame will do when it wears off in a non-oiled hole. Anyone?
    • Hi not found one either yet,  close relative is the 436 and 4361 according to ranff.db.   It gives quire a lot of detail but not as good as the old site.      RANFF.DB.
    • No problem to replace the setting with the staking set. Press the new setting from inside, use flat face punch with hole. The punch must be wider than the setting, the hole to be as not to press at the stone, but only on the bush. Press by hand until the setting gets flush with the plate surface, so the punch must rest on it.
    • Yes, the arbor usually makes about 3 to 3.5 turns. But usually spring takes 2/3 to 3/4 of the free space in barrel, not 1/2, so take it for the calcullations. This way the change in torque is smaller. I have a picture for You, this one is little older, but no mater
    • I overhauled a ladies Rolex and noticed erratic performance so I stripped in down again and did fault finding. This is what I saw. The lower jewel (the one in the plate) is cracked and the hole is too big. Before discovering this, I stripped down and re-cleaned the main-plate (and parts) by hand with a fine natural fiber brush. I somehow missed the fault the first time and cannot understand how it was still running. Perhaps re-cleaning it dislodged some pieces of the jewel widening the hole? I don't know. Now I need to replace the jewel but don't have a Seitz tool. The Rolex part is 2130-0913 and the top and bottom are the same. The part comes complete in brass setting with KIF elastor spring and cap jewel. Note: I have never replaced a jewel. I do have a good vintage stacking set that I've used quite a bit.  Can I replace using a stacking set? Any suggestions would be greatly appreciated.  
×
×
  • Create New...