For really dirty parts, put them in a small jar filled with cleaning solution then put that jar into the ultrasonic filled with water.

That way you dont contaminate litres of cleaning solution.



Keep replacing the solution in the jar until it doesn't change colour or you are happy with the cleanliness of the parts inside it.
Link to comment
Share on other sites

Not ultra-sonic but I have a spare set of jars for my cleaning machine.

Whenever I change the cleaning solutions the old stuff goes into the spare jars specifically for use as a pre-clean on the really grotty movements.

Usually a very dirty movement goes in whole prior to disassembly and goes through a complete wash/rinse/dry cycle in the old chemistry before I break it down to component level for a proper clean in the fresh stuff.

This not only helps to get the most out of the cleaning fluids but it can also help to ease the disassembly process, even helping to free up really tight or stuck screws.

  • Like 1
Link to comment
Share on other sites

That's one reason you may want to limit how long because it becomes hot...but somehow not too hot to cause what CB describes if the chemicals are used at room temperature (by the time they get too hot, the process is already over so to speak)...I suppose we are talking about a "regular" ultrasonic, not a home brewed one...

The chemicals could be an issue if they are not the "customary" ones for this application, since alcohol based chemicals will act on the shellac in addition of being flammable. Flammable chemicals are not recommended for ultrasonics.

  • Like 1
Link to comment
Share on other sites

6 hours ago, szbalogh said:

My aim is to remove hard gummed oils

I think you're going to find that hard gummy oil conceivably may never come off especially in pivots which is why you're supposed to use peg wood.

Then commercial cleaning fluids are made out of variety of substances one of which is used to brighten the plates so they come out nice and shiny. That is a really nice but leave it into long and you start etching plates. This is why typically I won't go over five minutes with ultrasonic cleaning and the solution. It does depend upon temperature if the solutions hot it's going to be much more aggressive.

Then alcohol and shellac they're all a little different. The machine at work the last two rinses are isopropyl alcohol it seems to have zero effect on shellac. I use wood alcohol at home but limit the exposure to just a few seconds as the very very final rinse.They change the formula of the commercial rinse I was using and it didn't seem to want to dry as fast even with heat so a final final rinse of alcohol and I had no problems with that.

Then when working on pocket watches especially old pocket watches always check the jewels afterwards anyway. The shellac will become old possibly with time and sometimes it's not shellac. The longer the watches had exposure to a variety of repair people the more creative they've gotten so it's always good to check to make sure the jewels are still in place.

 

  • Like 1
Link to comment
Share on other sites

2 hours ago, JohnR725 said:

I think you're going to find that hard gummy oil conceivably may never come off especially in pivots which is why you're supposed to use peg wood.

Then commercial cleaning fluids are made out of variety of substances one of which is used to brighten the plates so they come out nice and shiny. That is a really nice but leave it into long and you start etching plates. This is why typically I won't go over five minutes with ultrasonic cleaning and the solution. It does depend upon temperature if the solutions hot it's going to be much more aggressive.

Then alcohol and shellac they're all a little different. The machine at work the last two rinses are isopropyl alcohol it seems to have zero effect on shellac. I use wood alcohol at home but limit the exposure to just a few seconds as the very very final rinse.They change the formula of the commercial rinse I was using and it didn't seem to want to dry as fast even with heat so a final final rinse of alcohol and I had no problems with that.

Then when working on pocket watches especially old pocket watches always check the jewels afterwards anyway. The shellac will become old possibly with time and sometimes it's not shellac. The longer the watches had exposure to a variety of repair people the more creative they've gotten so it's always good to check to make sure the jewels are still in place.

 

Thank you! Currently i dont have commercial cleaning fluid, used benzine from the pharmacy instead. The plates are not siny. 

At first disasdembly i had to pull hard on the escape wheel, it was so hard gummed. Now the escape wheel bridge jewel is nice clean. So this ultrabath is an awsome equipment. 

The watch however running currently without oil -10 min a day. I will demagnetize and repair the hairspring's bent terminal curve and if all is set will strip it again for a second ultrabath.

Got a blower ball today and used tried it on the wet parts. It is so good that i had blown the clickspring away... couldnt find it.

Edited by szbalogh
Link to comment
Share on other sites

51 minutes ago, szbalogh said:

benzine from the pharmacy

The next time you're at the pharmacy ask what the health differences between the exposure to benzine or benzene? Noticed two different spellings there actually two different substances. Both are used as solvents one of them as extremely bad health consequences on exposure to. Just make sure the version you're using doesn't have the same bad health consequences

One of the problems with hobbyists for cleaning fluid is it may be hard to get. The problem becomes the variety of solvents art always a good substitute for the commercial cleaning fluids and the wrong choice could have consequences.

Then cleaning and rinse isn't exactly technically correct. The entire process is cleaning. The cleaning fluids have a variety of chemicals to dissolve the lubrication brighten the plates hopefully put everything in the solution so it comes off the parts. The rinse is actually a continuation of the cleaning process just a diluting the concentration of the chemicals found in the cleaner. So at the very end of your cleaning process all the bad stuff is hopefully been removed everything is clean.

  • Like 2
Link to comment
Share on other sites



  • Recently Browsing

    • No registered users viewing this page.
  • Topics

  • Posts

    • So that is what the last person to work on this movement appears to have done.  There was a "wad" of adhesive material in the vicinity of that hole when I took the dial off.  I was hoping to take the high road and fix the issue in the work I did on this movement. I wasn't sure if I was imagining things or not when I looked at the screw hole, but it does appear to be somewhat distended.  I had not considered the posibility that someone had forced a screw that too big in there.  I had wondered about using a technique I've applied in other applications (where the screws are in the same scale as human hands) that involves counter drilling the plug with a  reverse threaded tap.  When I've had to do that in the past, the screw has generally caught and backed out from the torque on the tap (instead of yielding and letting the tap bore into it.)  I don't like doing that, but it's saved my rear a couple of times, but the smallest bolt I've tried that on had a 5 mm head.  This is an entirely different ball of wax. I am still contemplating disolving the screw with alum, even if that means I have to stick the dial down with double sided tape until I gain the skills to actually replace the screw.
    • Hi Thomas, you should be able to find the right (or on close to beeing) in a Ronda or DCN balance staff catalogue. Cousins uk have those available as a download.
    • Hello everyone. My name is Cees (pronounced "case"). I have been working on watches for a few years now. Got down the rabbit hole when I started watching "how to" videos on watch repair when my watch broke while on holiday. I'm not interested in collecting watches, but purely in the technical side. I love fixing them and also love collecting the tools I need (or might possibly need one day...).
    • The movement is FHF, something like this. But it will not help much to find stem.  Sometimes making one is easier
    • I think they all have their pros and cons, the one I suggested is a threadlock loctite product (Loctite is now owned by Henkel), In general I use the current one that is recommended on their Loctite page (link here)   I use blue (243) for the actual crown the (stick is actually 248 which is the stick version of 243), like I said it is very convenient for using on stems. Blue holds the crown for everyday use, but can be removed if you need to with a little heat. I use the red 277 for things like stem extensions where I have no intention of ever removing it. The purple I don't use (but I have seen some youtubers use it) as I think the blue is removable so why take the risk on a weaker product.   This is interesting, and a useful bit of information to know 🙂
×
×
  • Create New...