Barrel bushing


nickelsilver

Recommended Posts

I have a nice little carriage clock in for service, very good shape, except for over 0.30mm sideshake of the barrel arbor in the barrel. Thought I would show how I bush these; it seems they often get overlooked or just skipped as they are a little more fussy than just bushing a plate. I measure everything up, then remove the boss in the barrel, and make a bushing that fits from the inside and is stepped, replacing the boss. This way it's captive, and doesn't require a big interference fit to get seated and stay. I turn up the bushing with a boring tool in the lathe, doing the outside as well (running in reverse of course), then do the barrel opening with the same tool. It's a pretty quick process once you have the moves down!

 

 

20191022_115827 (Large).jpg

20191022_120745 (Large).jpg

20191022_121316 (Large).jpg

20191022_121500 (Large).jpg

20191022_121734 (Large).jpg

20191022_122442 (Large).jpg

  • Like 5
Link to comment
Share on other sites

How did I miss this? I always let the bush protrude by a tiny amount on the face side, then clean off, that way by the time you have finished cleaning up and polishing the barrel you wouldn’t see the bush. Nevertheless a good tidy job. We all have our own ways of working.  

images.jpg

Link to comment
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.
Note: Your post will require moderator approval before it will be visible.

Guest
Reply to this topic...

×   Pasted as rich text.   Restore formatting

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.



  • Recently Browsing

    • No registered users viewing this page.
  • Topics

  • Posts

    • When faced with say a pocket watch bridge which is cracked, silver soldering to repair is often the only option (hopefully someone wasn't there before hand with soft solder). I can generally do this succesfully and tidily with a small torch and miniscule pieces of silver solder, but on parts which were mercury amalgam gilded the heat can have have a deleterious effect on the finish.   I keep wondering if there's a good way to refinish these - and despite having the needful items would rather avoid using the mercury process.   In the past for electronic work I've gold plated PCBs but this involved gold potassium cyanide solution, which also doesn't realy belong at home. I've read that there are now safer alternatives but couldn't find more detail (and importantly how similar are the results to amalgam gilding, since I wouldn't want to refinish the whole watch). Pointers would be very welcome (and yes, I know solutions containing gold won't be cheap!) Alan
    • The first one is an Unruh max stake for pushing out staffs
    • Ok so with the great answers for my previous question may I ask what these two attachments are used for. The one with the red knob is I assume used for hand setting the seconds hand? Jon      
    • According to Cousins site I need to look at document G22 as I think I need an ATGB at 304 but I cant find this size in G22 doc. The last thing I want to do is order the wrong one😳  Unless I cant see the wood for the trees 😆 I could be looking at the wrong style, I assume its classed as Round plastic Armed  https://www.cousinsuk.com/product/wide-ring-gold-atgb
    • When building a new Watch I have tended to use a file to remove the remnants of dial feet that are not needed as many dials come with four feet to accomodate different movements, but this can be a bit messy so now I use this with a great deal more precision as you can use an appropriate bit for the job and keep it very localised.      
×
×
  • Create New...