So I recently serviced a 15 jewel Waltham Export grade 16s movement and it has these beautiful gold colored plate screws etc. What is the correct terminology for these? Would they be considered gilt? I know blued hands tend to be more common but I'm sure there must be a term for this color of finish. Thank you for any info you can provide!

Screenshot_20230303-115913.png

Link to comment
Share on other sites

unhelpful answer is its heat-treated. If you look at a heat treating chart there is a temperature range where you get a gold color and my understanding and that's what this is. I've seen a number of watches that do this. I even had an Elgin watch where all the screws of course were gold and the hairspring was gold. Which did give don't remember what but it did have some different timing characteristics because instead of being a blued steel spring it's a gold steel spring which of course is going to have different physical properties

then can't read your serial number but you might look on the pocket watch database and see if it says anything.

.

https://pocketwatchdatabase.com/

 

 

  • Thanks 1
Link to comment
Share on other sites

13 minutes ago, JohnR725 said:

unhelpful answer is its heat-treated. If you look at a heat treating chart there is a temperature range where you get a gold color and my understanding and that's what this is. I've seen a number of watches that do this. I even had an Elgin watch where all the screws of course were gold and the hairspring was gold. Which did give don't remember what but it did have some different timing characteristics because instead of being a blued steel spring it's a gold steel spring which of course is going to have different physical properties

then can't read your serial number but you might look on the pocket watch database and see if it says anything.

.

https://pocketwatchdatabase.com/

 

 

I thought the colours indicated the temperature not the final colour ?

Link to comment
Share on other sites

1 hour ago, RichardHarris123 said:

I thought the colours indicated the temperature not the final colour ?

When tempering the steel it aquires a hue of colour. Different tones indicate a different level of temper. Wood chisels i used to harden to a cherry red quench in water then temper to a purple or blue maybe cant quite remember and then dip in sand or leave to air cool. I think , long time ago memory is fuzzy today. 

Link to comment
Share on other sites

3 hours ago, JohnR725 said:

unhelpful answer is its heat-treated. If you look at a heat treating chart there is a temperature range where you get a gold color and my understanding and that's what this is. I've seen a number of watches that do this. I even had an Elgin watch where all the screws of course were gold and the hairspring was gold. Which did give don't remember what but it did have some different timing characteristics because instead of being a blued steel spring it's a gold steel spring which of course is going to have different physical properties

then can't read your serial number but you might look on the pocket watch database and see if it says anything.

.

https://pocketwatchdatabase.com/

 

 

Ok this is very helpful thank you! Wow sounds like a very cool Elgin movement.

Link to comment
Share on other sites

1 minute ago, RichardHarris123 said:

I still don't see how heat treatment alone gives a gold colour. 

Exactly the same a "bluing" but to a lower temperature. (e.g. https://www.youtube.com/watch?v=AeISVhZxLm8 )

It's a thin oxide layer which causes the colour by interreference.

You need precise temp control to get a steady yellow - I've only blued.

Link to comment
Share on other sites

7 minutes ago, mikepilk said:

Exactly the same a "bluing" but to a lower temperature. (e.g. https://www.youtube.com/watch?v=AeISVhZxLm8 )

It's a thin oxide layer which causes the colour by interreference.

You need precise temp control to get a steady yellow - I've only blued.

Does it have to be cooled at a specific rate? 

Link to comment
Share on other sites

if you're doing screws today the easiest way is with some of the electric hot plates. you can dial an exact temperatures and get exact colors without going past. Unlike heating it up the traditional way if you're not careful you can easily go past where you need to be.

  • Like 1
Link to comment
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.
Note: Your post will require moderator approval before it will be visible.

Guest
Reply to this topic...

×   Pasted as rich text.   Restore formatting

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.



  • Recently Browsing

    • No registered users viewing this page.
  • Topics

  • Posts

    • So I found what I believe is the setting lever screw! Am I right in thinking the screw next to the click is the correct one for the setting lever? However if it is, it doesn't fit in the hole which I believe is for it! I can get the lever to sit nicely on the stem and line up with a hole, but the screw only goes as far as the shoulder and stops. It's as though the hole is too small! The dial side has been disassembled by the way, the other wheels are in my tray
    • When faced with say a pocket watch bridge which is cracked, silver soldering to repair is often the only option (hopefully someone wasn't there before hand with soft solder). I can generally do this succesfully and tidily with a small torch and miniscule pieces of silver solder, but on parts which were mercury amalgam gilded the heat can have have a deleterious effect on the finish.   I keep wondering if there's a good way to refinish these - and despite having the needful items would rather avoid using the mercury process.   In the past for electronic work I've gold plated PCBs but this involved gold potassium cyanide solution, which also doesn't realy belong at home. I've read that there are now safer alternatives but couldn't find more detail (and importantly how similar are the results to amalgam gilding, since I wouldn't want to refinish the whole watch). Pointers would be very welcome (and yes, I know solutions containing gold won't be cheap!) Alan
    • The first one is an Unruh max stake for pushing out staffs
    • Ok so with the great answers for my previous question may I ask what these two attachments are used for. The one with the red knob is I assume used for hand setting the seconds hand? Jon      
    • According to Cousins site I need to look at document G22 as I think I need an ATGB at 304 but I cant find this size in G22 doc. The last thing I want to do is order the wrong one😳  Unless I cant see the wood for the trees 😆 I could be looking at the wrong style, I assume its classed as Round plastic Armed  https://www.cousinsuk.com/product/wide-ring-gold-atgb
×
×
  • Create New...