I have this Tag that is getting a new crystal.  (My neighbor discovered my hobby!)  I ordered a generic 24mm by 2mm from Ofrei because this is what I measured of the broken crystal and the inner diameter of the watch.  I measured before removing the crystal and then after removing, I pieced together to confirm.

I have watched the WRT video on this topic, so I think I understand.

When the crystal arrives, I am going to use my crystal press and push!

When using the press, I will use the correct adapters so that the movement sits planar to the press.

If there is any special consideration due to it being a Tag, please let me know.

I bought two crystals because...well...it is my first time ?

Edited by LittleWatchShop
Link to comment
Share on other sites

  • LittleWatchShop changed the title to Tag Heuer crystal glass replacement guidance
14 hours ago, LittleWatchShop said:

 I ordered a generic 24mm by 2mm from Ofrei because this is what I measured of the broken crystal and the inner diameter of the watch. 

That works if the crystal is flat without bevels, but an expensive watch it may have some subtle features. And even if the original was mineral glass I'd recommend to the owner to fit a sapphire one. 

The measurement is made with the crystal removed, to inner diameter of the gasket. 

Link to comment
Share on other sites



  • Recently Browsing

    • No registered users viewing this page.
  • Topics

  • Posts

    • When faced with say a pocket watch bridge which is cracked, silver soldering to repair is often the only option (hopefully someone wasn't there before hand with soft solder). I can generally do this succesfully and tidily with a small torch and miniscule pieces of silver solder, but on parts which were mercury amalgam gilded the heat can have have a deleterious effect on the finish.   I keep wondering if there's a good way to refinish these - and despite having the needful items would rather avoid using the mercury process.   In the past for electronic work I've gold plated PCBs but this involved gold potassium cyanide solution, which also doesn't realy belong at home. I've read that there are now safer alternatives but couldn't find more detail (and importantly how similar are the results to amalgam gilding, since I wouldn't want to refinish the whole watch). Pointers would be very welcome (and yes, I know solutions containing gold won't be cheap!) Alan
    • The first one is an Unruh max stake for pushing out staffs
    • Ok so with the great answers for my previous question may I ask what these two attachments are used for. The one with the red knob is I assume used for hand setting the seconds hand? Jon      
    • According to Cousins site I need to look at document G22 as I think I need an ATGB at 304 but I cant find this size in G22 doc. The last thing I want to do is order the wrong one😳  Unless I cant see the wood for the trees 😆 I could be looking at the wrong style, I assume its classed as Round plastic Armed  https://www.cousinsuk.com/product/wide-ring-gold-atgb
    • When building a new Watch I have tended to use a file to remove the remnants of dial feet that are not needed as many dials come with four feet to accomodate different movements, but this can be a bit messy so now I use this with a great deal more precision as you can use an appropriate bit for the job and keep it very localised.      
×
×