Jump to content

Recommended Posts

Might be my second long winded post for today ( apologies if i bore anyone ( tough ).  So one of the many problems that crops up when buying cheap watches on ebay is wear to case plating. Often a good movement and dial on a watch can be sidestepped  because we dont have a fully workable item. And then its only use is as a donor, thats another vintage watch that bites the dust ( thanks for the quote G ). It is one of the issues that puts us off buying an otherwise good watch. Should that be the case ? ( excuse the pun ) How difficult can it be ? As far as i know, no its not especially hard to do, yet its not that often discussed as a topic. There is some info in the forum archives, but i thought it might be an idea to bring it up again for refreshment, something for beginners to think about and food for thought for others. Maybe its just me i dont know but i think every watch deserves a chance to be brought back to life. Some of these early vintage watches were not cheap in their day, if you owned  a nice watch in our grandparents day you had money or you worked bloody hard to get it. So my educated assumptions lead me to believe a lot of these watches were cherished gifts. Sad to see them sold off for peanuts 😪. My empathy side has got the better of me with this one, so I'm wanting to fully restore every watch i pick up and give them back the love that they once received and were used to express.  ( Yes i am a fanny,  what of it ) 😆. So the tool geek that i am and wanting to do things proper like, i have treat myself to this little number. An electric current outputter ?  My next step is to decide on the type of plating to apply. Something hard-wearing,  easy to work with , not expensive to buy but provides a reasonable finish and polishes well. Hopefully this little blog encourages others to give it a whirl and save a few old timers in the process.  Here is the unit i bought, it was pretty cheap. 

20220726_093722.jpg

  • Like 2
Link to comment
Share on other sites

2 hours ago, Neverenoughwatches said:

Might be my second long winded post for today ( apologies if i bore anyone ( tough ).  So one of the many problems that crops up when buying cheap watches on ebay is wear to case plating. Often a good movement and dial on a watch can be sidestepped  because we dont have a fully workable item. And then its only use is as a donor, thats another vintage watch that bites the dust ( thanks for the quote G ). It is one of the issues that puts us off buying an otherwise good watch. Should that be the case ? ( excuse the pun ) How difficult can it be ? As far as i know, no its not especially hard to do, yet its not that often discussed as a topic. There is some info in the forum archives, but i thought it might be an idea to bring it up again for refreshment, something for beginners to think about and food for thought for others. Maybe its just me i dont know but i think every watch deserves a chance to be brought back to life. Some of these early vintage watches were not cheap in their day, if you owned  a nice watch in our grandparents day you had money or you worked bloody hard to get it. So my educated assumptions lead me to believe a lot of these watches were cherished gifts. Sad to see them sold off for peanuts 😪. My empathy side has got the better of me with this one, so I'm wanting to fully restore every watch i pick up and give them back the love that they once received and were used to express.  ( Yes i am a fanny,  what of it ) 😆. So the tool geek that i am and wanting to do things proper like, i have treat myself to this little number. An electric current outputter ?  My next step is to decide on the type of plating to apply. Something hard-wearing,  easy to work with , not expensive to buy but provides a reasonable finish and polishes well. Hopefully this little blog encourages others to give it a whirl and save a few old timers in the process.  Here is the unit i bought, it was pretty cheap. 

20220726_093722.jpg

To add to this I've been trying  come up with ideas on what to use for plating anodes. Nickle is about the most popular material to use. As a yorkshire man ( yep you know whats coming 😉) and being tighter than the lid of a jar of pickled walnuts in grandma's hands . I am looking for alternative cheaper ( preferably nil ) supplies. My first thoughts were coins, new British coins are nickle plated steel, not sure how this would work. But experimentation will give me a good answer providing i dont blow myself up with my new gadget and a beaker full of electrolised  water. Somehow i cant get my head around using electricity and water at the same time in conjunction with each other. Next i was thinking zinc plating, tin cans ? . Copper plating ? Probably not, too quickly oxidises verdigris. The universe as always will provide me with an answer when i do good things. 👍 

Link to comment
Share on other sites

Most of the nice plating finishes like chrome, gold and rhodium, involve really toxic substances. Things that I wouldn't want in the house.

I tried nickel plating with a homemade electrolyte of nickel dissolved in vinegar. It doesn't give a very nice finish though.

I'm not sure if the problem is with the current density or with the electrode purity. The electrode was cut from a supposed pure nickel plate bought from AliExpress. 🤪

  • Like 1
Link to comment
Share on other sites

Getting the right voltage is key to get a good finish and is determined by the size of the piece to be plated and the concentration of the electrolyte. This will take a little experimentation. What you don’t want is bubbles forming, that will leave pit marks in the finish. But without bubbles, the reaction is painfully slow. So what worked for me was to manually stir the electrolyte just as bubbles started forming, it then gave a thick’ish, albeit dull finish, which brightened up nicely with a very fine polish.

This video helped:

 

  • Like 1
Link to comment
Share on other sites

7 hours ago, HectorLooi said:

Most of the nice plating finishes like chrome, gold and rhodium, involve really toxic substances. Things that I wouldn't want in the house.

I tried nickel plating with a homemade electrolyte of nickel dissolved in vinegar. It doesn't give a very nice finish though.

I'm not sure if the problem is with the current density or with the electrode purity. The electrode was cut from a supposed pure nickel plate bought from AliExpress. 🤪

Thank Hectori, appreciate your input . I will bere that in mind about the toxic stuff. If i suddenly disappear from the forum never to return you know whats happened 😆

2 hours ago, gbyleveldt said:

Getting the right voltage is key to get a good finish and is determined by the size of the piece to be plated and the concentration of the electrolyte. This will take a little experimentation. What you don’t want is bubbles forming, that will leave pit marks in the finish. But without bubbles, the reaction is painfully slow. So what worked for me was to manually stir the electrolyte just as bubbles started forming, it then gave a thick’ish, albeit dull finish, which brightened up nicely with a very fine polish.

This video helped:

 

Thanks Gert, i had an idea that the voltage and current was particularly important thats why I opted for a something with a good range and good adjustment. And i so love a good experiment, a bit like baking. My madeleines are to die for 😁. I will want to make some kind of auto stirrer then, i wonder if something to just slowly spin the case would work. Thanks for the video link Gert much appreciated.  I'll send you some of my baking as soon as i invent a space transporter. Or else a parcel of crumbs (  the Royal Mail is not what it used to be ). 

Link to comment
Share on other sites

2 hours ago, Neverenoughwatches said:

Thanks Gert, i had an idea that the voltage and current was particularly important thats why I opted for a something with a good range and good adjustment. And i so love a good experiment, a bit like baking. My madeleines are to die for 😁. I will want to make some kind of auto stirrer then, i wonder if something to just slowly spin the case would work. Thanks for the video link Gert much appreciated.  I'll send you some of my baking as soon as i invent a space transporter. Or else a parcel of crumbs (  the Royal Mail is not what it used to be ). 

Yeah, you'd be surprised how little voltage you need. I think on average it's between 1.5V and 2.0V, size depending. For the hands I did I just stirred it manually as it took less than a minute to plate nicely. I haven't done a whole case before but I'd imagine the voltage should be in a similar range based on other videos I've seen.

The fancy stirrers have a little oblong piece chucked into the electrolyte, then you put the whole lot on a "stirrer" that spins the piece through electromagnetism. Pretty neat; I believe these are pretty common from laboratory suppliers.

Hah, I'm not allowed anywhere near the kitchen because "I always make a mess". Put me behind a Grill and I'll cook up a storm though hehe. Pity about Royal mail (and South African mail to be honest), I'd love to critique your baking prowess!

  • Like 2
Link to comment
Share on other sites

4 hours ago, gbyleveldt said:

Yeah, you'd be surprised how little voltage you need. I think on average it's between 1.5V and 2.0V, size depending. For the hands I did I just stirred it manually as it took less than a minute to plate nicely. I haven't done a whole case before but I'd imagine the voltage should be in a similar range based on other videos I've seen.

The fancy stirrers have a little oblong piece chucked into the electrolyte, then you put the whole lot on a "stirrer" that spins the piece through electromagnetism. Pretty neat; I believe these are pretty common from laboratory suppliers.

Hah, I'm not allowed anywhere near the kitchen because "I always make a mess". Put me behind a Grill and I'll cook up a storm though hehe. Pity about Royal mail (and South African mail to be honest), I'd love to critique your baking prowess!

Thank you for that Gert. Any thoughts as to a zinc plate ? And just wondering how important the electrolyte concentration is and how to test it. I'm tempted to have a go tonight with nickel plated coins to see if it pulls the nickel from them. 

Link to comment
Share on other sites

2 hours ago, Neverenoughwatches said:

Thank you for that Gert. Any thoughts as to a zinc plate ? And just wondering how important the electrolyte concentration is and how to test it. I'm tempted to have a go tonight with nickel plated coins to see if it pulls the nickel from them. 

Hmmmm, that I'm not too sure about to be honest. In order to make electrolyte you'll have to have a pretty pure source of Nickel. I followed the instructions in the video above to make electrolyte. Apart from actual Nickel, you should have all the stuff at home. To make the electrolyte I did push about 15V into the solution for an hour or so, it actually got nice and warm. Once the electrolyte is made then you can re-use many times, but making it properly is pretty important

  • Like 1
Link to comment
Share on other sites

You can get nickel and zinc electrodes from AliExpress. 

SG$ 6.33  90%OFF | Pure Nickel 99.99% Plate Electrode 0.8mm X 25mm X 150mm Sacrificial Anode Plating Sheet
https://a.aliexpress.com/_mqEn9Si

SG$ 4.53  40%OFF | 1mm 2mm 3mm thick width 10mm length 100mm 5pcs/lot Zinc Sheet Plate Pure Metal Zinc Plate Foil for Science Lab Accessories
https://a.aliexpress.com/_mrJB0kw

  • Like 1
Link to comment
Share on other sites

5 hours ago, HectorLooi said:

You can get nickel and zinc electrodes from AliExpress. 

SG$ 6.33  90%OFF | Pure Nickel 99.99% Plate Electrode 0.8mm X 25mm X 150mm Sacrificial Anode Plating Sheet
https://a.aliexpress.com/_mqEn9Si

SG$ 4.53  40%OFF | 1mm 2mm 3mm thick width 10mm length 100mm 5pcs/lot Zinc Sheet Plate Pure Metal Zinc Plate Foil for Science Lab Accessories
https://a.aliexpress.com/_mrJB0kw

Thank you Hector. 

Link to comment
Share on other sites

  • 8 months later...

I have fairly good results with a home made nickel plate solution, but I think you need to be concentrating on maintaining constant amperage not voltage. When creating the plating solution I keep my amperage at 3.0A, but when plating I keep it at 0.1A - low and slow for plating a watch case seems to do the trick. You may also want to invest in a magnetic stirrer, they are relatively cheap and the agitation they create prevents bubbles forming on the watch case, and where there are bubbles there is no plating solution and then you get patchy plating. Here is the one I use:

 

image.thumb.png.97022c66e896d03a3162f0eaa07066a2.png

Also, remember to turn the watch case every so often so that each side faces the electrode and you get an even plate.

  • Like 2
Link to comment
Share on other sites

On 4/18/2023 at 10:07 AM, Waggy said:

I have fairly good results with a home made nickel plate solution, but I think you need to be concentrating on maintaining constant amperage not voltage. When creating the plating solution I keep my amperage at 3.0A, but when plating I keep it at 0.1A - low and slow for plating a watch case seems to do the trick. You may also want to invest in a magnetic stirrer, they are relatively cheap and the agitation they create prevents bubbles forming on the watch case, and where there are bubbles there is no plating solution and then you get patchy plating. Here is the one I use:

 

image.thumb.png.97022c66e896d03a3162f0eaa07066a2.png

Also, remember to turn the watch case every so often so that each side faces the electrode and you get an even plate.

Thanks for the information waggy. Instead of a stirrer i turn the case I'm plating via a small overhead adjustabe speed motor. 

  • Like 1
Link to comment
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.
Note: Your post will require moderator approval before it will be visible.

Guest
Reply to this topic...

×   Pasted as rich text.   Restore formatting

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.



  • Recently Browsing

    • No registered users viewing this page.
  • Topics

  • Posts

    • So I found what I believe is the setting lever screw! Am I right in thinking the screw next to the click is the correct one for the setting lever? However if it is, it doesn't fit in the hole which I believe is for it! I can get the lever to sit nicely on the stem and line up with a hole, but the screw only goes as far as the shoulder and stops. It's as though the hole is too small! The dial side has been disassembled by the way, the other wheels are in my tray
    • When faced with say a pocket watch bridge which is cracked, silver soldering to repair is often the only option (hopefully someone wasn't there before hand with soft solder). I can generally do this succesfully and tidily with a small torch and miniscule pieces of silver solder, but on parts which were mercury amalgam gilded the heat can have have a deleterious effect on the finish.   I keep wondering if there's a good way to refinish these - and despite having the needful items would rather avoid using the mercury process.   In the past for electronic work I've gold plated PCBs but this involved gold potassium cyanide solution, which also doesn't realy belong at home. I've read that there are now safer alternatives but couldn't find more detail (and importantly how similar are the results to amalgam gilding, since I wouldn't want to refinish the whole watch). Pointers would be very welcome (and yes, I know solutions containing gold won't be cheap!) Alan
    • The first one is an Unruh max stake for pushing out staffs
    • Ok so with the great answers for my previous question may I ask what these two attachments are used for. The one with the red knob is I assume used for hand setting the seconds hand? Jon      
    • According to Cousins site I need to look at document G22 as I think I need an ATGB at 304 but I cant find this size in G22 doc. The last thing I want to do is order the wrong one😳  Unless I cant see the wood for the trees 😆 I could be looking at the wrong style, I assume its classed as Round plastic Armed  https://www.cousinsuk.com/product/wide-ring-gold-atgb
×
×
  • Create New...